sarlink 22035N是一种高度工程化的热塑性硫化胶,也可作为复合母料,用于要求苛刻的汽车和工业应用。Sarlink 22035N是一种低硬度、低密度等级,具有优异的拉伸强度、优越的压缩永久变形、耐化学性和高温性能。它可以很容易地通过注射成型,吹塑或挤出加工各种应用,如靴子和波纹管,密封件,垫圈以及其他型材和物品。 Sarlink® 22035N is a highly engineered thermoplastic vulcanizate that can also be used as a compound masterbatch for use in demanding automotive and industrial applications. Sarlink® 22035N is a low hardness, low density grade with exceptional tensile strength, superior compression set, chemical resistance and high temperature performance. It can be easily processed by injection molding, blow molding or extrusion for various applications such as boots and bellows, seals, gaskets as well as other profiles and articles.
Sarlink TPV 5700B系列是高度工程化的挤出级热塑性硫化橡胶,具有出色的紫外线稳定性,适用于要求严格的汽车内外密封应用,包括玻璃槽、腰带、挡风雨条、密封件和其他型材。Sarlink® TPV X5735B是一种低硬度、低密度、高性能的产品,具有低雾化、优异的保色性和弹性。 The Sarlink TPV 5700B series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. Sarlink TPV X5735B is a low hardness, low density, high performance grade with low fogging and excellent color retention and elastic properties.
产品描述
厂家:
美国特诺尔爱佩斯 Teknor Apex
美国特诺尔爱佩斯 Teknor Apex
类别:
TPV TPV
TPV TPV
填料:
用途:
汽车领域的应用,密封件,等角速万向节防尘套,橡胶取代,型材,垫圈,工业应用
汽车外部零件,汽车领域的应用,橡胶取代
性能特点:
易加工,尺寸稳定性好,耐高温,拉伸性能好,低密度,硬度低,耐化学性 Excellent Processability,Good Dimensional Stability,High Heat Resistance,Good Tensile Strength,Low density,Low Hardness,Solvent resistance
耐候抗UV,易加工,有弹性,低密度,硬度低,耐化学性 Weather resistance is good,Excellent Processability,Elastic,Low density,Low Hardness,Solvent resistance
加工条件:
挤出 Extrusion
技术参数
物理性能 PHYSICAL
Sarlink® TPV 22035N
Sarlink® TPV X5735B
单位 UNIT
测试方法 TEST METHOD
密度
Density
g/cm³
ASTM D792
密度
Density
g/cm³
ISO 1183
弹性体 ELASTOMER
Sarlink® TPV 22035N
Sarlink® TPV X5735B
单位 UNIT
测试方法 TEST METHOD
压缩形变(125℃,70 hr)
Compression deformation
%
ASTM D395
压缩形变(125℃,70 hr)
Compression deformation
%
ISO 815
压缩形变(23℃,22 hr)
Compression deformation
%
ASTM D395
压缩形变(23℃,22 hr)
Compression deformation
%
ISO 815
压缩形变(70℃,22 hr)
Compression deformation
%
ASTM D395
压缩形变(70℃,22 hr)
Compression deformation
%
ISO 815
拉伸应变(断裂)
Tensile strain
%
ASTM D412
拉伸应变(断裂)
Tensile strain
%
ISO 37
拉伸应变(流量,断裂)
Tensile strain
%
ASTM D412
拉伸应变(流量,断裂)
Tensile strain
%
ISO 37
拉伸强度(MD,100% 应变)
tensile strength
MPa
ASTM D412
拉伸强度(MD,100% 应变)
tensile strength
MPa
ISO 37
拉伸强度(MD,断裂)
tensile strength
MPa
ASTM D412
拉伸强度(MD,断裂)
tensile strength
MPa
ISO 37
拉伸强度(TD,100% 应变)
tensile strength
MPa
ASTM D412
拉伸强度(TD,100% 应变)
tensile strength
MPa
ISO 37
拉伸强度(断裂)
tensile strength
MPa
ASTM D412
拉伸强度(断裂)
tensile strength
MPa
ISO 37
撕裂强度(TD)
tear strength
kN/m
ASTM D624
撕裂强度(TD)
tear strength
kN/m
ISO 34-1
机械性能 MECHANICAL
Sarlink® TPV 22035N
Sarlink® TPV X5735B
单位 UNIT
测试方法 TEST METHOD
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
ASTM D2240
邵氏硬度(邵氏 A,5 秒,挤出成型)
Shore hardness
ISO 868
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
ASTM D2240
邵氏硬度(邵氏 A,5 秒,注塑成型)
Shore hardness
ISO 868
老化性能 AGING
Sarlink® TPV 22035N
Sarlink® TPV X5735B
单位 UNIT
测试方法 TEST METHOD
体积变化(125℃,70 hr,在IRM 903油中)
Volume change
%
ASTM D471
体积变化(125℃,70 hr,在IRM 903油中)
Volume change
%
ISO 1817
在空气中断裂时拉伸应力变化 - TD(135℃,1000 hr)
Changes in tensile stress when fractured in air - TD
%
ISO 188
在空气中断裂时拉伸应力变化 - TD(150℃,168 hr)
Changes in tensile stress when fractured in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变 135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变 150℃,168 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(100% 应变,135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(100% 应变,150℃,168 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(135℃,1000 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
ASTM D573
空气中拉伸强度的变化率 - TD(150℃,168 hr)
Change rate of tensile strength in air - TD
%
ISO 188
空气中极限伸长率的变化率(135℃,1000 hr)
Change in Ultimate Elongation in Air
%
ASTM D573
空气中极限伸长率的变化率(150℃,168 hr)
Change in Ultimate Elongation in Air
%
ASTM D573
空气中硬度计硬度的变化率(邵氏 A,135℃,1000 hr)
Change in Durometer Hardness in Air
ASTM D573
空气中硬度计硬度的变化率(邵氏 A,150℃,168 hr)
Change in Durometer Hardness in Air
ASTM D573
空气中邵氏硬度的变化率(邵氏 A,135℃,1000 hr)
Change in Shore Hardness in Air
ISO 188
空气中邵氏硬度的变化率(邵氏 A,150℃,168 hr)
Change in Shore Hardness in Air
ISO 188
补充信息
Sarlink® TPV 22035N
Sarlink® TPV X5735B
单位 UNIT
测试方法 TEST METHOD
熔体表观粘度 - Capillary @ 206/s(200℃)
Apparent viscosity of melt - Capillary @ 206/s
Pa·s
ASTM D3835
熔体表观粘度 - Capillary @ 206/s(200℃)
Apparent viscosity of melt - Capillary @ 206/s
Pa·s
ISO 11443
熔体表观粘度 - Capillary,@ 206/s(200℃)
Apparent viscosity of melt - Capillary, @ 206/s
Pa·s
ASTM D3835
熔体表观粘度 - Capillary,@ 206/s(200℃)
Apparent viscosity of melt - Capillary, @ 206/s
Pa·s
ISO 11443