Glastic® 1580是一种易于制造的层压板,具有优异的阻燃性。该阻燃层压板符合保险商实验室的UL94V0规范。这种材料最初是为满足电视行业的安全保证要求而设计的。Glastic® 1580具有优异的阻燃性、抗电弧性和高温能力,适用于反激变压器和电弧堆组件等应用。 Glastic 1580 is an easily fabricated laminate that exhibits excellent flame resistance. This flame-resistant laminate meets the UL94 V0 specification of Underwriters Laboratories. This material was originally designed to meet the television industry's safety assurance requirements. Glastic 1580 has exceptional flame resistance, arc resistance and a high temperature capability for applications such as flyback transformers and arc stack assemblies. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.83 | g/cm³ | ASTM D792 |
吸水率 Water Absorption |
|||
24hr 24hr |
0.20 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength |
|||
屈服,1.60 mm Yield, 1.60 mm |
57.9 | MPa | ASTM D638 |
弯曲强度 Flexural Strength |
|||
屈服,1.60 mm Yield, 1.60 mm |
170 | MPa | ASTM D790 |
压缩强度 compressive strength |
|||
1.60 mm 1.60 mm |
215 | MPa | ASTM D695 |
剪切强度 shear strength |
MPa | ASTM D732 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
悬臂梁缺口冲击强度 Izod Notched Impact strength |
|||
1.6mm 1.6mm |
J/m | ASTM D256 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
线性热膨胀系数 Coeff.of linear therm expansion |
|||
MD:1.6 mm MD:1.6 mm |
1/℃ | ASTM D696 | |
导热系数 Thermal Conductivity |
W/m/K | ASTM C177 | |
相对温度指数 Relative temperature index |
|||
电气性能,1.60 mm Electrical performance, 1.60 mm |
℃ | UL 746 | |
1.60 mm 1.60 mm |
℃ | UL 746 | |
电气性能 ELECTRICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
介电强度 Dielectric strength 1 |
ASTM D149 | ||
1.6 mm,在空气中 1.6 mm in air |
kV/mm | ASTM D149 | |
1.6 mm,在油中 1.6 mm in oil |
kV/mm | ASTM D149 | |
耗散因数 Dissipation factor |
ASTM D150 | ||
1.60 mm,60 Hz 1.60 mm,60 Hz |
ASTM D150 | ||
1.60 mm,1 MHz 1.60 mm,1 MHz |
ASTM D150 | ||
耐电弧性 Arc resistance |
|||
1.60 mm 1.60 mm |
sec | ASTM D495 | |
相比耐漏电起痕指数 Compared to the resistance to leakage and marking index |
|||
1.60 mm 1.60 mm |
V | UL 746 | |
高电弧燃烧指数(HAI)(1.60 mm) High Arc Burning Index (HAI) (1.60 mm) |
UL 746 | ||
热丝引燃(HWI)(1.60 mm) Hot wire ignition (HWI) (1.60 mm) |
sec | UL 746 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
1.60 mm 1.60 mm |
UL 94 | ||
极限氧指数 Oxygen Index |
|||
1.6 mm 1.6 mm |
% | ASTM D2863 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 方法A(短时间) |
【新闻资讯】查看全部 ![]()
【干货】如何解决塑件表面光泽不良?
2021-03-04 搜料网资讯: 什么是表面光泽不良 ? 光泽不良是指表面昏暗没有光泽,透明制品的透明性低下,造成光泽不良的原因很多,其他的一些注塑缺陷也是造成光泽不良的原因。 表面光泽不 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |