公司信息及水印






牌号简介 About |
---|
Riblene® FF 30是一种高分子量低密度聚乙烯(LDPE),适用于吹塑薄膜挤出。Riblene® FF 30的特点是具有良好的熔融强度,在挤压过程中具有良好的气泡稳定性。Riblene® FF 30制造的薄膜容易热收缩,具有良好的光学和机械性能。主要用途Riblene® FF 30推荐用于生产中轻负荷收缩膜、层压膜和混合膜。 Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterised by a good melt strength leading to a good bubble stability during extrusion. Films manufactured by Riblene FF 30 are easily heat shrinkable and characterised by good optical and mechanical properties. Main Application Riblene FF 30 is recommended for the production of shrink film for medium and light loads, for lamination film and for blend. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.923 | g/cm³ | ISO 1183 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
0.80 | g/10min | ISO 1133 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
摩擦系数 Frictional coefficient |
|||
与自身 - 动态,吹塑薄膜 Self dynamic, blow molded film |
> 0.50 | ISO 8295 | |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
70 | µm | |
薄膜厚度 film thickness |
30 to 120 µm | ||
拉伸模量 Tensile modulus |
ISO 527-3 | ||
1% 正割,MD,70 µm,吹塑薄膜 1% secant, MD, 70 µ m, blow molded film |
MPa | ISO 527-3 | |
1% 正割,TD,70 µm,吹塑薄膜 1% secant, TD, 70 µ m, blow molded film |
MPa | ISO 527-3 | |
拉伸强度 tensile strength |
ISO 527-3 | ||
MD,屈服,70 µm,吹塑薄膜 MD, yield, 70 µ m, blow molded film |
MPa | ISO 527-3 | |
TD,屈服,70 µm,吹塑薄膜 TD, yield, 70 µ m, blow molded film |
MPa | ISO 527-3 | |
拉伸强度 tensile strength |
ISO 527-3 | ||
MD,断裂,70 µm,吹塑薄膜 MD, fracture, 70 µ m, blow molded film |
MPa | ISO 527-3 | |
TD,断裂,70 µm,吹塑薄膜 TD, fracture, 70 µ m, blow molded film |
MPa | ISO 527-3 | |
拉伸应变 Tensile strain |
ISO 527-3 | ||
MD,断裂,70 µm,吹塑薄膜 MD, fracture, 70 µ m, blow molded film |
% | ISO 527-3 | |
TD,断裂,70 µm,吹塑薄膜 TD, fracture, 70 µ m, blow molded film |
% | ISO 527-3 | |
落锤冲击 Gardner Impact 2 |
|||
70 µm,吹塑薄膜 70 µ m, blow molded film 2 |
g | ISO 7765-1/A | |
埃尔曼多夫抗撕强度 Elmandorf tear strength 3 |
ISO 6383-2 | ||
MD:70.0 µm MD:70.0 µm |
kN/m | ISO 6383-2 | |
TD:70.0 µm TD:70.0 µm |
kN/m | ISO 6383-2 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
脆化温度 Brittle Temperature |
℃ | ASTM D746 | |
维卡软化温度 Vicat Softening Temperature |
℃ | ISO 306/A | |
熔融温度 Melting temperature |
℃ | 内部方法 | |
光学性能 OPTICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45°,70 µm,吹塑薄膜 45 °, 70 µ m, blow molded film |
ASTM D2457 | ||
雾度 Haze |
|||
70.0 µm,吹塑薄膜 70.0 µ m, blow molded film |
% | ISO 14782 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 F50 |
3 Blown Film |
【新闻资讯】查看全部 ![]()
德方数据显示,中国取代美国成为德机械制造业最大出口市场
2021-05-21 搜料网资讯: 记者20日从德国联邦外贸与投资署(GTAI)获悉,根据德国机械设备制造业联合会(VDMA)发布的最新数据,今年第一季度德国在机械制造领域向中国出口额增长(同比,下同)20.3%, |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |