公司信息及水印






牌号简介 About |
---|
30%玻璃纤维增强阻燃聚酰胺PA66,注塑成型。 TECHNYL® A 60G1 V30 Natural is a polyamide 66 based on a non-halogenated flame retardant system, reinforced with 30% of glass fiber, heat stabilized, for injection moulding. This grade offers excellent flame retardancy properties (UL 94, 5VA, GWIT) combined with excellent processing, mechanical and electrical performance. It can withstand temperatures of 160°C for over 6000 hours and has a UL F1 rating for weatherability resistance |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.46 | g/cm³ | ISO 1183/A |
吸水率 Water Absorption |
|||
饱和,23℃ Saturation, 23 ℃ |
4.3 | % | ISO 62 |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
1.8 | % | ISO 62 |
23℃,24hr 23℃,24hr |
0.73 | % | ISO 62 |
耐候性 Weathering resistance |
f1 | UL 746C | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
MPa | ISO 527-2/1A | |
拉伸强度 tensile strength |
|||
断裂,23℃ Fracture, 23 ℃ |
MPa | ASTM D638 | |
断裂,23℃ Fracture, 23 ℃ |
MPa | ISO 527-2/1A | |
拉伸应变 Tensile strain |
|||
断裂,23℃ Fracture, 23 ℃ |
% | ASTM D638 | |
断裂,23℃ Fracture, 23 ℃ |
% | ISO 527-2 | |
弯曲模量 Flexural Modulus |
|||
23℃ 23℃ |
MPa | ISO 178 | |
23℃ 23℃ |
MPa | ASTM D790 | |
弯曲强度 Flexural Strength |
|||
23℃ 23℃ |
MPa | ASTM D790 | |
23℃ 23℃ |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
ISO 179/1eA | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eA | |
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotched Impact strength |
ISO 179/1eU | ||
-30℃ -30℃ |
kJ/m² | ISO 179/1eU | |
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
悬臂梁缺口冲击强度 Izod Notched Impact strength |
|||
23℃ 23℃ |
J/m | ASTM D256 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 HDT |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/Af | |
熔融温度 Melting temperature |
℃ | ISO 11357-3 | |
电气性能 ELECTRICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
0.8 mm 0.8 mm |
kV/mm | IEC 60243-1 | |
相比漏电起痕指数 Comparative Tracking Index |
|||
解决方案 A Solution A |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame Class Rating |
UL 94 | ||
0.80 mm 0.80 mm |
UL 94 | ||
1.60 mm 1.60 mm |
UL 94 | ||
3.20 mm 3.20 mm |
UL 94 | ||
灼热丝可燃性指数 Glow Wire Flammability Index(GWFI) |
IEC 60695-2-12 | ||
0.80 mm 0.80 mm |
℃ | IEC 60695-2-12 | |
1.6 mm 1.6 mm |
℃ | IEC 60695-2-12 | |
3.2 mm 3.2 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Glow Wire Ignitability Temperature(GWIT) |
|||
0.8 mm 0.8 mm |
℃ | IEC 60695-2-13 | |
极限氧指数 Oxygen Index |
% | ISO 4589-2 | |
French Fire Index French Fire Index |
NF F16-101 | ||
French Smoke Index French Smoke Index |
NF F16-101 | ||
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
欧洲铁路认证 European Railway Certification |
EN 45545-2 | ||
R22 R22 |
EN 45545-2 | ||
R23 R23 |
EN 45545-2 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部 ![]()
【干货】怎样做好注塑工艺?
2020-11-30 搜料网资讯: 现今加工工艺的趋势正朝着高新技术的方向发展,这些技术包括:微型注塑、高填充复合注塑、水辅注塑、混合使用各种特别注塑成型工艺、泡沫注塑、模具技术、仿真技 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |