产品描述:trexprene A88NU是一种热稳定的PP/EPDM基热塑性硫化弹性体(TPV)。这种天然化合物主要用于发动机罩下的应用,如垫子、密封件、垫圈、风管、CVJ护套、盖子、索环或其他需要柔软性和一致性的零件。这种材料可以使用注塑、挤压、吹塑或其他熔融加工技术进行加工。 Product Description: TREXPRENE ® A88NU is a heat stabilized PP/EPDM based Thermoplastic Vulcanized Elastomer (TPV). This Natural compound is intended primarily for underhood applications such as mats, seals, gaskets, air ducts, CVJ boots, covers, grommets or other parts where softness and conformity are needed. This material can be processed using Injection Molding, Extrusion, Blow Molding or other melt processing techniques. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.930 到 0.990 | g/cm³ | ISO 1183 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
邵氏硬度 Shore hardness |
|||
邵氏 A,15 秒 Shore A, 15 seconds |
86 到 92 | ISO 868 | |
弹性体 Elastomer |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸强度 tensile strength 1 |
|||
TD,屈服 TD, yield 2 |
12.3 | MPa | ISO 37 |
TD,100% 应变 TD, 100% strain 1 |
6.50 | MPa | ISO 37 |
拉伸应变 Tensile strain 3 |
|||
TD,断裂 TD, fracture 3 |
710 | % | ISO 37 |
撕裂强度 tear strength 4 |
|||
TD TD 4 |
kN/m | ISO 34-1 | |
压缩形变 Compression deformation |
|||
125℃,70 hr 125℃,70 hr |
% | ASTM D395B | |
125℃,70 hr 125℃,70 hr 5 |
% | ISO 815 | |
老化性能 Aging property |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
空气中拉伸强度的变化率 Change in Tensile Strength in Air |
ISO 188 | ||
135℃,1000 hr 135℃,1000 hr |
% | ||
150℃,168 hr 150℃,168 hr |
% | ||
在空气中断裂时拉伸应力变化 Change in Tensile Strain at Break in Air |
ISO 188 | ||
135℃,1000 hr 135℃,1000 hr |
% | ||
150℃,168 hr 150℃,168 hr |
% | ||
拉伸强度的变化率 Change in Tensile Strength |
|||
125℃,70 hr,在IRM 903油中 125 ℃, 70 hr, in IRM 903 oil |
% | ISO 1817 | |
断裂时拉伸应力变化 Change in tensile stress during fracture |
|||
125℃,70 hr,在IRM 903油中 125 ℃, 70 hr, in IRM 903 oil |
% | ISO 1817 | |
体积变化 Volume change |
|||
125℃,70 hr,在 IRM 903 油中 125 ℃, 70 hr, in IRM 903 oil |
% | ISO 1817 | |
撕裂强度的变化率 Change rate of tear strength |
|||
70 hrs,in IRM 903 Oil,125℃ 70 hrs,in IRM 903 Oil,125℃ |
% | ISO 1817 | |
Change in Tensile Properties Change in Tensile Properties |
|||
Stress at 100% Elongation in Air,168 hrs:150℃ Stress at 100% Elongation in Air,168 hrs:150℃ |
% | ISO 188 | |
Stress at 100% Elongation in IRM 903 Oil,70 hrs:125℃ Stress at 100% Elongation in IRM 903 Oil,70 hrs:125℃ |
% | ISO 1817 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
脆化温度 Brittle Temperature |
|||
-- -- |
℃ | ASTM D746 | |
类型 B Type B |
℃ | ISO 812 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
燃烧速率 Burning Speed |
mm/min | ISO 3795 | |
补充信息 Supplementary information |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
耐臭氧性 Ozone resistance 6 |
|||
40℃ 40℃ 6 |
ISO 1431-1 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 类型 1, 20 in/min |
3 B 方法,直角形试样(不割口), 20 in/min |
4 类型 A |
5 100 pphm, Method A |
【新闻资讯】查看全部
塑料净化严重,回收再利用非常紧急
2018-06-14 塑料可说是人类又爱又恨的朋友,带来方便的同时,也对地球造成难以挽回伤害,世界经济论坛(WEF)曾预测,假如再不落实塑料回收或减产,2050 年海洋塑料会比鱼还要多。 根据 Science Advances 研究,截至 2015 年,在美国共约 63 亿公吨塑料垃圾中,只有 9% 落实回收,剩下 12% 进焚化炉、约 79% 塑料最后归宿在垃圾掩埋场或随意丢弃。即使是拥有严格废弃物管理制度的欧洲国家,也只有 31% 塑料回收再利用,因此不少学者认为,如果无法好好回收塑料,那就 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |