Noryl NH7114树脂是一种20%的玻璃增强改性PPE-PS混合物。该材料使用非卤化阻燃剂,以达到UL94的火焰等级,同时提供了一个特殊的强度和尺寸稳定性平衡。这一等级可以通过挤压或注射成型加工。诺丽尔NH7114可定制颜色,可能是一个优秀的材料候选人在电气和电子市场使用。 NORYL NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of strength and dimensional stability. This grade can be processed via extrusion or injection molding. NORYL NH7114 is available in custom colors and may be an excellent material candidate for use in electrical and electronics markets. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.25 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
280℃,5.0kg 280℃,5.0kg |
5.8 | g/10min | ASTM D1238 |
熔体体积流动速率 Melt Volume Rate |
|||
300℃,5 kg 300℃,5 kg |
10.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage |
|||
MD:3.2 mm MD:3.2 mm |
0.20 到 0.30 | % | 内部方法 |
吸水率 Water Absorption |
|||
饱和,23℃ Saturation, 23 ℃ |
0.22 | % | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ||
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
-- -- 3 |
MPa | ASTM D638 | |
-- -- |
MPa | ISO 527-1-2 | |
拉伸强度 tensile strength |
|||
屈服 yield 4 |
MPa | ASTM D638 | |
屈服 yield |
MPa | ISO 527-2/5 | |
断裂 fracture 4 |
MPa | ASTM D638 | |
断裂 fracture |
MPa | ISO 527-2/5 | |
拉伸应变 Tensile strain |
|||
屈服 yield 4 |
% | ASTM D638 | |
屈服 yield |
% | ISO 527-2/5 | |
断裂 fracture 4 |
% | ASTM D638 | |
断裂 fracture |
% | ISO 527-2/5 | |
弯曲模量 Flexural Modulus |
|||
50 mm跨距 50 mm span 5 |
MPa | ASTM D790 | |
-- -- 6 |
MPa | ISO 178 | |
弯曲强度 Flexural Strength |
|||
-- -- 6 , 7 |
MPa | ISO 178 | |
屈服,50 mm跨度 Yield, 50 mm span 5 |
MPa | ASTM D790 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength 8 |
|||
23℃ 23℃ 8 |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotched Impact strength 8 |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
悬臂梁缺口冲击强度 Izod Notched Impact strength |
|||
-30℃ -30℃ |
J/m | ASTM D256 | |
23℃ 23℃ |
J/m | ASTM D256 | |
-30℃ -30℃ 9 |
kJ/m² | ISO 180-1A | |
23℃ 23℃ 9 |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Izod Unnotched Impact strength 9 |
|||
-30℃ -30℃ |
kJ/m² | ||
23℃ 23℃ |
kJ/m² | ||
装有测量仪表的落镖冲击 Dart impact equipped with measuring instruments |
|||
23℃,Total Energy 23℃,Total Energy |
J | ASTM D3763 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 HDT |
|||
1.8 MPa,未退火,3.2 mm 1.8 MPa, unannealed, 3.2 mm |
℃ | ASTM D648 | |
1.8 MPa,未退火,4.0 mm,64 mm跨距 1.8 MPa, unannealed, 4.0 mm, 64 mm span 9 |
℃ | ISO 75-2/Af | |
维卡软化温度 Vicat Softening Temperature |
|||
-- -- |
℃ | ASTM D1525 10 | |
B120 B120 |
℃ | ISO 306/B120 | |
球压测试 Ball pressure test |
|||
123~127℃ 123~127℃ |
IEC 60695-10-2 | ||
线性热膨胀系数 Coeff.of linear therm expansion |
|||
MD:-40~40℃ MD:-40~40℃ |
1/℃ | ASTM E831 | |
TD:-40~40℃ TD:-40~40℃ |
1/℃ | ASTM E831 | |
TD:-40℃ TD:-40℃ |
1/℃ | ISO 11359-2 | |
相对温度指数 Relative temperature index |
℃ | UL 746 | |
电气性能 ELECTRICAL |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
℃ | UL 746 | |
电气性能 ELECTRICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
3.2 mm,在油中 3.2 mm in oil |
kV/mm | ASTM D149 | |
3.2 mm,在油中 3.2 mm in oil |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant |
|||
1 MHz 1 MHz |
ASTM D150 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
|||
1 MHz 1 MHz |
ASTM D150 | ||
相比漏电起痕指数 Comparative Tracking Index |
UL 746 | ||
高电弧燃烧指数(HAI) High Arc Burning Index (HAI) 11 |
UL 746 | ||
高压电弧抗点燃指数(HVAR)(PLC) High voltage arc ignition resistance index (HVAR) (PLC) |
UL 746 | ||
高电压电弧起痕速率 High Voltage Arc Track Rate |
|||
HVTR HVTR |
UL 746 | ||
热丝引燃 Hot wire ignition |
|||
HWI HWI |
UL 746 | ||
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame Class Rating |
|||
1.50 mm 1.50 mm |
|||
6.00 mm 6.00 mm |
|||
2.00 mm 2.00 mm |
|||
灼热丝可燃性指数 Glow Wire Flammability Index(GWFI) |
|||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Glow Wire Ignitability Temperature(GWIT) |
|||
1 mm 1 mm |
℃ | ||
2 mm 2 mm |
℃ | ||
极限氧指数 Oxygen Index |
% | ISO 4589-2 |
备注 |
---|
3. 5.0 mm/min |
4. 类型 1, 5.0 mm/min |
5. 1.3 mm/min |
6. 2.0 mm/min |
7. at Yield |
8. 80*10*4 sp=62mm |
9. 80*10*4 mm |
10. 速率 A (50°C/h), 载荷2 (50N) |
11. Surface |
【新闻资讯】查看全部
雀巢是第一家参与Project STOP的食品公司
2019-01-17 近日,前沿倡导项目Project STOP(Stop Ocean Plastics)宣布雀巢将成为其新战略合作伙伴,预防塑料碎片流入东南亚海洋。 据悉,雀巢是第一家加入Project STOP的食品公司,其合作伙伴还包括北欧化工(Borealis)、SYSTEMIQ,以及来自挪威政府的合作伙伴诺瓦化学(NOVA Chemicals),博禄(Borouge)和威立雅(Veolia)。 雀巢全球运营主管Magdi Batato说:“我们很高兴成为第一家加入Pro |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |