公司信息及水印








牌号简介 About |
---|
Ultradur® B 4300 G4是一种易于流动的注射成型PBT,具有20%的玻璃纤维增强,用于刚性、坚固和尺寸稳定的零件。典型应用包括车门把手、小电机外壳、前照灯夹持器和制动鼓控制器。 Ultradur B 4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. Applications Typical applications include car door handles, housings for small electric motors, headlight retainers and drum controllers. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.45 | g/cm³ | ASTM D792 |
密度 Density |
1.45 | g/cm³ | ISO 1183 |
熔体体积流动速率 Melt Volume Rate |
|||
250℃,2.16 kg 250℃,2.16 kg |
14.0 | cm³/10min | ISO 1133 |
收缩率 Shrinkage |
ISO 294-4 | ||
MD:3.2 mm MD:3.2 mm |
0.40 | % | |
TD TD |
1.2 | % | ISO 294-4 |
MD MD |
% | ISO 294-4 | |
吸水率 Water Absorption |
|||
饱和,23℃ Saturation, 23 ℃ |
% | ISO 62 | |
饱和 saturated |
% | ASTM D570 | |
平衡,23℃,50% RH Equilibrium, 23 ℃, 50% RH |
% | ISO 62 | |
平衡,50% RH Balance, 50% RH |
% | ASTM D570 | |
粘度值 Viscosity value |
|||
降低的粘度 Reduced viscosity |
ml/g | ISO 1628 | |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
|||
23℃ 23℃ |
MPa | ISO 527-2 | |
拉伸强度 tensile strength |
ISO 527-2 | ||
断裂,23℃ Fracture, 23 ℃ |
MPa | ASTM D638 | |
断裂,-40℃ Fracture, -40 ℃ |
MPa | ISO 527-2 | |
断裂,23℃ Fracture, 23 ℃ |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
ISO 527-2 | ||
断裂,23℃ Fracture, 23 ℃ |
% | ASTM D638 | |
断裂,-40℃ Fracture, -40 ℃ |
% | ISO 527-2 | |
断裂,23℃ Fracture, 23 ℃ |
% | ISO 527-2 | |
弯曲模量 Flexural Modulus |
|||
23℃ 23℃ |
MPa | ASTM D790 | |
23℃ 23℃ |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179 | |
简支梁无缺口冲击强度 Charpy Unnotched Impact strength |
ISO 179 | ||
-30℃ -30℃ |
kJ/m² | ISO 179 | |
23℃ 23℃ |
kJ/m² | ISO 179 | |
悬臂梁缺口冲击强度 Izod Notched Impact strength |
|||
23℃ 23℃ |
J/m | ASTM D256 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 HDT |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ASTM D648 | |
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ISO 75-2/B | |
0.45 MPa,未退火 0.45 MPa, unannealed |
℃ | ASTM D648 | |
熔融峰值温度 Melting peak temperature |
℃ | ASTM D3418 | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | ISO 3146 | |
线性热膨胀系数 Coeff.of linear therm expansion |
|||
MD MD |
1/℃ | ||
相对温度指数 Relative temperature index |
|||
电气性能 ELECTRICAL |
UL 746 | ||
0.75 mm 0.75 mm |
℃ | UL 746 | |
1.5 mm 1.5 mm |
℃ | UL 746 | |
3.0 mm 3.0 mm |
℃ | UL 746 | |
强度机械性能 Strength mechanical performance |
UL 746 | ||
0.75 mm 0.75 mm |
℃ | UL 746 | |
1.5 mm 1.5 mm |
℃ | UL 746 | |
3.0 mm 3.0 mm |
℃ | UL 746 | |
冲击机械性能 Impact mechanical performance |
UL 746 | ||
0.75 mm 0.75 mm |
℃ | UL 746 | |
1.5 mm 1.5 mm |
℃ | UL 746 | |
3.0 mm 3.0 mm |
℃ | UL 746 | |
电气性能 ELECTRICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
1.5 mm 1.5 mm |
ohms | ASTM D257 | |
体积电阻率 Volume resistivity |
ohms·cm | IEC 60093 | |
1.50 mm 1.50 mm |
ohms·cm | ASTM D257 | |
介电常数 Dielectric constant |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
耗散因数 Dissipation factor |
IEC 60250 | ||
100 Hz 100 Hz |
IEC 60250 | ||
1 MHz 1 MHz |
IEC 60250 | ||
相比漏电起痕指数 Comparative Tracking Index |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame Class Rating |
UL 94 | ||
1.50 mm 1.50 mm |
UL 94 | ||
3.00 mm 3.00 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
【新闻资讯】查看全部
倍耐力轮胎采用银胶菊做橡胶资料
2015-12-25 近日,倍耐力首次使用源自植物银胶菊的天然橡胶生产超高性能轮胎,并在维佐拉和巴洛科测试赛道使用玛莎拉蒂Ghibli成功试跑。这种非粮食作物在干旱气候中非常典型,可以在无农药和少水的条件下培育,因而可以成为橡胶树的替代品。 这款创新的概念胎创记录地只用了两年时间,就从最初的原材料研究到了实体赛道试跑。2013年时,倍耐力与意大利石化巨头Eni集团旗下化工企业Versalis公司签订协议,由对方独家供应银胶菊天然橡胶,用于轮胎生产。在极短的周期内,倍耐力的研发人员在实验室环境下深 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |