| 牌号简介 About |
|---|
| iRogran A95K 4640是一种基于己内酯的热塑性聚氨酯。该材料已开发用于注射成型应用,要求在压缩永久变形、耐磨性和抗水解性能方面优于传统的聚酯基TPU。iRogran A95K 4640是高性能注塑产品系列的一部分,提供一种特殊设计的柔性材料,适用于生产密封件、车轮和辊、耦合半轴和O形圈。性能特点:高耐磨性、低压缩永久变形、短循环时间、优异的抗水解性、高动态负荷 IROGRAN A95K 4640 is a caprolactone-based thermoplastic polyurethane. The material has been developed for injection molding applications requiring exceptional performance in terms of compression set, wear resistance and hydrolysis resistance over conventional polyester-based TPUs. IROGRAN A95K 4640 is part of the High Performance Injection Molding product range and offers a specially designed, flexible material suitable for the production of seals, wheels and rollers, coupling halfs and o-rings. PERFORMANCE FEATURES High wear resistance Low compression set Short cycle times Excellent hydrolysis resistance Resistant to high dynamic loads |
| 技术参数 Technical Data | |||
|---|---|---|---|
|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
|
密度 Density 2 |
1.19 | g/cm³ | ASTM D792 |
|
密度 Density 3 |
1.19 | g/cm³ | DIN 53479 |
|
熔体体积流动速率 Melt Volume Rate |
|||
|
210℃,2.16 kg 210℃,2.16 kg |
5.00 to 10.0 | cm³/10min | |
|
收缩率 Shrinkage |
|||
|
MD:注塑成型 MD: Injection molding |
注册或登录后
所有资料免费
|
% | ASTM D972 |
|
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
|
邵氏硬度 Shore hardness |
注册或登录后
所有资料免费
|
ASTM D2240 | |
|
邵氏 A,注塑成型 Shaw A, injection molding |
注册或登录后
所有资料免费
|
ASTM D2240 | |
|
邵氏 D,注塑成型 Shaw's D, injection molding |
注册或登录后
所有资料免费
|
ASTM D2240 | |
|
邵氏硬度 Shore hardness |
注册或登录后
所有资料免费
|
DIN 53505 | |
|
邵氏 A,注塑成型 Shaw A, injection molding |
注册或登录后
所有资料免费
|
DIN 53505 | |
|
邵氏 D,注塑成型 Shaw's D, injection molding |
注册或登录后
所有资料免费
|
DIN 53505 | |
|
磨耗量 Wear amount 2 |
注册或登录后
所有资料免费
|
||
|
-- -- |
注册或登录后
所有资料免费
|
mm³ | ASTM D395 |
|
-- -- |
注册或登录后
所有资料免费
|
mm³ | DIN 53516 |
|
弹性体 Elastomer |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
|
拉伸强度 tensile strength 2 |
注册或登录后
所有资料免费
|
||
|
断裂 fracture 2 |
注册或登录后
所有资料免费
|
MPa | ASTM D412 |
|
断裂 fracture 2 |
注册或登录后
所有资料免费
|
MPa | DIN 53504 |
|
300% 应变 300% strain 2 |
注册或登录后
所有资料免费
|
MPa | ASTM D412 |
|
300% 应变 300% strain 2 |
注册或登录后
所有资料免费
|
MPa | DIN 53504 |
|
200% 应变 200% strain 2 |
注册或登录后
所有资料免费
|
MPa | ASTM D412 |
|
200% 应变 200% strain 2 |
注册或登录后
所有资料免费
|
MPa | DIN 53504 |
|
20% 应变 20% strain 2 |
注册或登录后
所有资料免费
|
MPa | ASTM D412 |
|
20% 应变 20% strain 2 |
注册或登录后
所有资料免费
|
MPa | DIN 53504 |
|
100% 应变 100% strain 2 |
注册或登录后
所有资料免费
|
MPa | ASTM D412 |
|
100% 应变 100% strain 2 |
注册或登录后
所有资料免费
|
MPa | DIN 53504 |
|
50% 应变 50% strain |
注册或登录后
所有资料免费
|
MPa | ASTM D412 |
|
50% 应变 50% strain |
注册或登录后
所有资料免费
|
MPa | DIN 53504 |
|
拉伸应变 Tensile strain 2 |
注册或登录后
所有资料免费
|
||
|
断裂 fracture 2 |
注册或登录后
所有资料免费
|
% | ASTM D412 |
|
断裂 fracture 2 |
注册或登录后
所有资料免费
|
% | DIN 53504 |
|
撕裂强度 tear strength 2 |
注册或登录后
所有资料免费
|
kN/m | ASTM D624 |
|
撕裂强度 tear strength 2 |
注册或登录后
所有资料免费
|
kN/m | DIN 53515 |
|
压缩形变 Compression deformation 2 |
注册或登录后
所有资料免费
|
ASTM D395 | |
|
23℃,24 hr 23℃,24 hr |
注册或登录后
所有资料免费
|
% | ASTM D395 |
|
70℃,24 hr 70℃,24 hr |
注册或登录后
所有资料免费
|
% | ASTM D395 |
|
100℃,24 hr 100℃,24 hr |
注册或登录后
所有资料免费
|
% | ASTM D395 |
|
100℃,70 hr 100℃,70 hr |
注册或登录后
所有资料免费
|
% | ASTM D395 |
|
压缩形变 Compression deformation 2 |
注册或登录后
所有资料免费
|
DIN 53517 | |
|
23℃,24 hr 23℃,24 hr |
注册或登录后
所有资料免费
|
% | DIN 53517 |
|
70℃,24 hr 70℃,24 hr |
注册或登录后
所有资料免费
|
% | DIN 53517 |
|
100℃,24 hr 100℃,24 hr |
注册或登录后
所有资料免费
|
% | DIN 53517 |
|
100℃,70 hr 100℃,70 hr |
注册或登录后
所有资料免费
|
% | DIN 53517 |
|
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
|
维卡软化温度 Vicat Softening Temperature 2 |
注册或登录后
所有资料免费
|
℃ | DIN 53372 |
| 备注 |
|---|
| 1 一般属性:这些不能被视为规格。 |
| 2 Injection Molded |
|
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |