AFFINITY*HT1285G聚烯烃塑性体(POP)是专门设计的高性能密封剂,适用于要求苛刻的包装应用。亲和力HT 1285G通过提高热粘强度、增强填缝性、通过污染获得优良密封性和低温密封启动,提供高包装完整性。它有助于使密封包装在今天的高速包装线或要求基板,并支持减少密封剂失效和潜在的相关食品浪费。亲和力HT 1285G已开发用于铸造、吹塑和挤出涂膜生产线的加工。柔性包装中的高完整性密封层低密封起始温度优良的热粘强度优良的味道和气味轮廓优良的密封通过污染符合:美国食品和药物管理局FCN 424欧盟,2011年第10号,完整细节请参考法规。 AFFINITY* HT1285G Polyolefin Plastomer (POP) is specifically designed as a high performance sealant for demanding packaging applications. AFFINITY HT 1285G provides high packaging integrity through improved hot tack strength, enhanced caulkability, superior seal though contamination, and low temperature seal initiation. It helps enable hermetic packaging on today's high speed packaging lines or with demanding substrates, and supports reducing sealant failure and potential related food waste. AFFINITY HT 1285G has been developed for processing on Cast, Blown, and Extrusion Coating film production lines. High integrity sealant layer in flexible packaging Low seal initiation temperature Excellent hot tack strength Excellent taste and odor profile Superior seal through contamination Complies with: U.S. FDA FCN 424 EU, No 10/2011 Consult the regulations for complete details. |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
0.898 | g/cm³ | ASTM D792 |
熔体质量流动速率 Melt Flow Rate |
|||
190℃,2.16kg 190℃,2.16kg |
6.0 | g/10min | ASTM D1238 |
薄膜 film |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
薄膜厚度 film thickness |
|||
测试 test |
25 | µm | |
拉伸强度 tensile strength |
ASTM D882 | ||
MD,屈服,25 µm MD, yield, 25 µ m |
5.80 | MPa | ASTM D882 |
TD,屈服,25 µm TD, yield, 25 µ m |
5.30 | MPa | ASTM D882 |
MD,断裂,25 µm MD, fracture, 25 µ m |
MPa | ASTM D882 | |
TD,断裂,25 µm TD, fracture, 25 µ m |
MPa | ASTM D882 | |
拉伸应变 Tensile strain |
ASTM D882 | ||
MD,断裂,25 µm MD, fracture, 25 µ m |
% | ASTM D882 | |
TD,断裂,25 µm TD, fracture, 25 µ m |
% | ASTM D882 | |
落锤冲击 Gardner Impact |
|||
25 µm 25 µm |
g | ASTM D1709-A | |
埃尔曼多夫抗撕强度 Elmandorf tear strength 2 |
ASTM D1922 | ||
MD:25 µm MD:25 µm |
g | ASTM D1922 | |
TD:25 µm TD:25 µm |
g | ASTM D1922 | |
始封温度 Initial sealing temperature |
℃ | ASTM D1525 | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
维卡软化温度 Vicat Softening Temperature |
℃ | ASTM D1525 | |
熔融温度 Melting temperature |
|||
DSC DSC |
℃ | 内部方法 | |
光学性能 OPTICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
光泽度 gloss |
|||
45°,25 µm,铸造薄膜 45 °, 25 µ m, cast thin film |
ASTM D2457 | ||
雾度 Haze |
|||
25 µm,铸造薄膜 25 µ m, cast thin film |
% | ASTM D1003 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 Method B |
【新闻资讯】查看全部 ![]()
车用聚丙烯资料“以塑代钢”已是大势所趋
2018-07-23 近几年,环保法规的监管日趋严谨,汽车向新能源转变成为必然,车用复合材料需求将不断增加,在汽车轻量化发展背景下,“以塑代钢”已是大势所趋。近期,三井化学公司计划将由日本Anesaki工厂生产玻璃纤维增强聚丙烯材料,以用于汽车内饰。该聚丙烯复材生产设施的设计产能为3500吨/年,计划于2019年9月完成。 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |