公司信息及水印








牌号简介 About |
---|
Amodel® A-4145 HH是一种45%玻璃纤维增强的热稳定级聚邻苯二甲酰胺(ppa),其设计目的是在230°C的温度下为热氧化降解提供优异的性能保持。其他特点是快速循环和热水可塑性。本产品特别适用于小尺寸汽车发动机的进气应用,如进气增压空气冷却和废气再循环。黑色:A-4145 HH BK324 Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation at temperatures of 230°C. Other features are fast cycling and hot water moldability. This product is particularly suitable to air induction applications within downsized automotive engines such as air induction charge air cooling and exhaust gas recirculation. Black: A-4145 HH BK324 |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.57 | g/cm³ | ISO 1183/A |
收缩率 Shrinkage |
|||
TD TD |
0.80 | % | ASTM D955 |
MD MD |
0.40 | % | ASTM D955 |
吸水率 Water Absorption |
|||
24hr 24hr |
0.37 | % | ASTM D570 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
16400 | MPa | ISO 527-2 |
拉伸强度 tensile strength |
ISO 527-2 | ||
断裂,23℃ Fracture, 23 ℃ |
MPa | ISO 527-2 | |
断裂,200℃ Fracture, 200 ℃ |
MPa | ISO 527-2 | |
断裂,230℃ Fracture, 230 ℃ |
MPa | ISO 527-2 | |
拉伸应变 Tensile strain |
ISO 527-2 | ||
断裂,23℃ Fracture, 23 ℃ |
% | ISO 527-2 | |
断裂,200℃ Fracture, 200 ℃ |
% | ISO 527-2 | |
断裂,230℃ Fracture, 230 ℃ |
% | ISO 527-2 | |
弯曲模量 Flexural Modulus |
|||
23℃ 23℃ |
MPa | ISO 178 | |
弯曲强度 Flexural Strength |
|||
23℃ 23℃ |
MPa | ISO 178 | |
压缩强度 compressive strength |
MPa | ASTM D695 | |
剪切强度 shear strength |
MPa | ASTM D732 | |
泊松比 Poisson's ratio |
ASTM E132 | ||
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
简支梁无缺口冲击强度 Charpy Unnotched Impact strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179/1eU | |
悬臂梁缺口冲击强度 Izod Notched Impact strength |
|||
23℃ 23℃ |
kJ/m² | ISO 180-1A | |
悬臂梁无缺口冲击强度 Izod Unnotched Impact strength |
|||
23℃ 23℃ |
kJ/m² | ISO 180/1U | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 HDT |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
熔融温度 Melting temperature |
℃ | ISO 11357-3 | |
熔融温度 Melting temperature |
℃ | ASTM D570 | |
线性热膨胀系数 Coeff.of linear therm expansion |
|||
TD TD |
ASTM E831 | ||
0 到 100℃ 0 to 100 ℃ |
cm/cm/℃ | ASTM E831 | |
100 到 200℃ 100 to 200 ℃ |
cm/cm/℃ | ASTM E831 | |
MD MD |
ASTM E831 | ||
0 到 100℃ 0 to 100 ℃ |
cm/cm/℃ | ASTM E831 | |
100 到 200℃ 100 to 200 ℃ |
cm/cm/℃ | ASTM E831 | |
电气性能 ELECTRICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
体积电阻率 Volume resistivity |
ohms·cm | ASTM D257 | |
介电强度 Dielectric strength |
|||
1.6 mm 1.6 mm |
kV/mm | ASTM D149 | |
介电常数 Dielectric constant |
ASTM D150 | ||
60 Hz 60 Hz |
ASTM D150 | ||
1 MHz 1 MHz |
ASTM D150 | ||
耗散因数 Dissipation factor |
ASTM D150 | ||
60 Hz 60 Hz |
ASTM D150 | ||
1 MHz 1 MHz |
ASTM D150 | ||
相比漏电起痕指数 Comparative Tracking Index |
V | UL 746 | |
高电压电弧起痕速率 High Voltage Arc Track Rate |
|||
HVTR HVTR |
mm/min | UL 746 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame Class Rating 2 |
|||
3.20 mm 3.20 mm |
UL 94 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 These flammability ratings are not intended to reflect hazards presented by these or any other materials under actual fire conditions. |
【新闻资讯】查看全部 ![]()
环氧树脂:“不平凡”的一年,反弹收官!
2022-01-05 搜料网资讯: 12月最后一周,液体树脂市场先跌后涨,固体树脂则顺势而为,受双酚A价格回升提振下于周五报盘拉涨。周内双原料涨跌互现,其中双酚A价格低位回升,环氧氯丙烷则继续 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |