牌号简介 About |
---|
EMERGE™ PC 8731HH高级树脂是一种阻燃的玻璃增强聚碳酸酯树脂。这种树脂不含溴、氯或磷酸盐添加剂。它是一种具有模具释放系统的中流量PC树脂,具有紫外线稳定功能,适用于注塑应用。Emerge PC 8731HH的UL 94 V-0额定值为1.5 mm。应用:电力设施[智能]仪表结构件 EMERGE™ PC 8731HH Advanced Resin is an ignition-resistant, glass reinforced, polycarbonate resin. This resin contains no bromine, chlorine, or phosphate additives. It is a medium flow PC resin with a mold release system and is UV stabilised, - intended for injection molding applications. EMERGE ™ PC 8731HH has a UL 94 V-0 rating at 1.5 mm. Applications: Electrical Utility [Smart] Meters Structural parts |
技术参数 Technical Data | |||
---|---|---|---|
物理性能 PHYSICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
密度 Density |
1.28 | g/cm³ | ISO 1183/B |
熔体质量流动速率 Melt Flow Rate |
|||
300℃,1.20kg 300℃,1.20kg |
8.0 | g/10min | ISO 1133 |
收缩率 Shrinkage |
0.40 到 0.60 | % | ISO 294-4 |
机械性能 MECHANICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
拉伸模量 Tensile modulus |
4350 | MPa | ISO 527-2/50 |
拉伸强度 tensile strength |
|||
屈服 yield |
85.0 | MPa | ISO 527-2/50 |
拉伸应变 Tensile strain |
|||
断裂 fracture |
% | ISO 527-2/50 | |
弯曲模量 Flexural Modulus 2 |
MPa | ISO 178 | |
弯曲强度 Flexural Strength 2 |
MPa | ISO 178 | |
冲击性能 IMPACT |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
简支梁缺口冲击强度 Charpy Notched Impact Strength |
|||
23℃ 23℃ |
kJ/m² | ISO 179/1eA | |
悬臂梁缺口冲击强度 Izod Notched Impact strength |
|||
23℃ 23℃ |
kJ/m² | ISO 180-A | |
热性能 THERMAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
热变形温度 HDT |
|||
1.8 MPa,未退火 1.8 MPa, unannealed |
℃ | ISO 75-2/A | |
维卡软化温度 Vicat Softening Temperature |
|||
B50 B50 |
℃ | ISO 306 | |
球压温度 Ball pressure temperature |
℃ | IEC 60598-1 | |
线性热膨胀系数 Coeff.of linear therm expansion |
|||
MD MD |
1/℃ | ISO 11359-2 | |
电气性能 ELECTRICAL |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
表面电阻率 Surface resistivity |
ohms | IEC 60093 | |
体积电阻率 Volume resistivity |
|||
2 mm 2 mm |
ohms·cm | IEC 60093 | |
介电强度 Dielectric strength |
|||
2 mm 2 mm |
kV/mm | IEC 60243-1 | |
介电常数 Dielectric constant 3 |
|||
2.00 mm 2.00 mm 3 |
IEC 60250 | ||
耗散因数 Dissipation factor 3 |
IEC 60250 | ||
相比漏电起痕指数 Comparative Tracking Index |
|||
3.00 mm,解决方案 A 3.00 mm, solution A |
V | IEC 60112 | |
阻燃性能 FLAME CHARACTERISTICS |
额定值 Nominal Value |
单位 Units |
测试方法 Test Method |
阻燃等级 Flame Class Rating 4 |
|||
1.50 mm 1.50 mm |
UL 94 | ||
灼热丝可燃性指数 Glow Wire Flammability Index(GWFI) 5 |
IEC 60695-2-12 | ||
1.0 mm 1.0 mm |
℃ | IEC 60695-2-12 | |
2.0 mm 2.0 mm |
℃ | IEC 60695-2-12 | |
3.0 mm 3.0 mm |
℃ | IEC 60695-2-12 | |
灼热丝起燃温度 Glow Wire Ignitability Temperature(GWIT) 4 |
IEC 60695-2-13 | ||
1 mm 1 mm |
℃ | IEC 60695-2-13 | |
2 mm 2 mm |
℃ | IEC 60695-2-13 | |
3 mm 3 mm |
℃ | IEC 60695-2-13 | |
极限氧指数 Oxygen Index 4 |
% | ISO 4589-2 |
备注 |
---|
1 一般属性:这些不能被视为规格。 |
2 0.079 in/min |
3 50 Hz to 1 MHz |
4 这个额定值并非为了反映这种或任何其他材料在实际起火条件下造成的危险。 |
5 This rating not intended to reflect hazards presented by this or any other material under actual fire conditions. |
【新闻资讯】查看全部 ![]()
【干货】背压对注塑成型有怎样的影响?
2021-05-10 搜料网资讯: 背压对注塑成型的作用是非常重要的,直接影响熔体的充模和塑件的质量。 (1)适当的背压可以提高制品的质量 ①能将炮筒内的熔料压实,增加密度,提高射胶量、制品 |
【免责声明】 广州搜料信息技术有限公司保留所有权利。 此数据表中的信息由搜料网soliao.com从该材料的生产商处获得。搜料网soliao.com尽最大努力确保此数据的准确性。 但是搜料公司对这些数据值及建议等给用户带来的不确定因素和后果不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。 |